recoat times, decrease recoat times, drying, drying times
No. Rust Bullet products do not contain lead, zinc, chromates, acids, or heavy metals.
The most accurate way to measure dry film thickness (DFT) is to use a DFT gauge. Apply an appropriate number of coats to achieve the desired DFT for the appropriate protection for your project. Immediately after application, measure the wet film thickness (WFT) with a WFT […]
Dry Film Thickness (DFT) is the thickness of a coating when dry, expressed in mils. One mil is equal to one thousandth of an inch. 1 mil = .001 inch (1/1000). For comparison purposes, the thickness of one sheet of standard paper is approximately 3-4 mils […]
Pleas see attached video for demonstration.
Yes, Rust Bullet coatings can be used on wood applications. Rust Bullet products provide a durable, protective layer that can help prevent deterioration caused by moisture, mold, and mildew. Here are a few considerations and steps to follow when using Rust Bullet on wood: Using Rust […]
curving outward, curving, convex
administer, employ, handle, use
The exact balance of viscosity, solvent, and active ingredients must be maintained; therefore, Rust Bullet coatings should never be mixed with any other products. Mixing another coating or adding any other unapproved product to a Rust Bullet coating will compromise the performance and quality of the […]
All Rust Bullet coatings come in a gloss or satin finish, and we have not found any flattening agent that is compatible with our coatings that do not effect its performance. At this time, we do not have a matte/flat finish option, nor do we have […]
Try to use a paint key, not a screwdriver. If the lid is still stuck, hammer the plug back into place and try prying it again. If that still doesn’t work, strike the plug dead center and it will release, every time.Here is a video illustration […]
Care should be taken to ensure that previously opened containers or left-over partial containers are kept sealed during storage. Rust Bullet coatings are moisture sensitive; limit the time the container is opened. During application, pour out the portion that will be used in approximately one hour […]
There are several issues to consider when painting over fiberglass, especially if there has been an existing failing paint. One issue is the application of a new coating system over an older, failing coating and another is the application on a very delicate and porous surface.Remove […]
Wait approximately one hour before applying a topcoat over the final coat of Rust Bullet Industrial or Rust Bullet Automotive that has been accelerated with Rapid Fire. The previous coat should be tack free.IMPORTANT: A Rust Bullet coating that has not been accelerated by adding Rapid […]
wash, toxin, discharge, dribble, empty, flow, overflow pour run out scatter, spill over, splash, spray, sprinkle, squirt, stream
care, caution, insurance, protection, provision, safeguard, safety measure, surface
Fossil fuels, such as refined oils (gasoline, diesel, jet fuels and kerosene) will not affect the integrity of a cured Rust Bullet coating. Additionally, renewable fuels such as Biodiesel and Ethanol will have no adverse effect on substrates coated with Rust Bullet.
Rust should not be coming to the surface unless Rust Bullet was improperly applied. Wipe down the coated surface with Rust Bullet Solvent and inspect the surface to rule out the possibility that the rust stains are caused by rusty water or fluid that has dripped […]
The drying time between coats of Rust Bullet is approximately two to six hours. If 12 or more hours have lapsed, wait for Rust Bullet to harden for at least 24 hours then lightly scuff with 80-100 grit sandpaper; enough to break the glaze to create […]
jar, glass, can, paint can, bag, bottle, canister, jug, pail, pot, storage
Rust Bullet coatings are ready to use right from the can. Due to the exact balance of viscosity, solvent, and active ingredients, it is not recommended to thin Rust Bullet coatings. If you have been advised by Rust Bullet to thin your product, it is important […]
If it is made of iron or steel, it will rust and corrode if left unprotected. Rust Bullet should be applied even where rust is not apparent to prevent the occurrence of future corrosion. Rust Bullet not only kills existing rust, but it also seals and […]
suggestion, suggestions, hints, warning
airless sprayer, HVLP sprayer
• Do not open Rust Bullet coatings until ready to use to maintain product shelf life.• Do not open and stir a Rust Bullet coating when the temperature is below the dew point.• Rust Bullet coatings should be stirred thoroughly for at least three minutes or […]
Both the Industrial and Automotive formulations have the same patented anti-corrosive properties and will outperform any other rust inhibitive, protective coating on the market. Rust Bullet Automotive is formulated to easily flow through an HVLP automotive spray system and will produce a smoother finish typically needed […]
Rust Bullet Industrial and Rust Bullet Automotive are super-tough, high-performance, industrial grade coatings that can be applied on new, clean metal or directly over surface rust, providing permanent corrosion protection with phenomenal adhesion. Rust Bullet has been awarded an unprecedented two U.S. patents by the United […]
Rust Bullet’s Application Guidelines are included with every order and can also be found on our Application and Technical Documents page. For the best possible results, it is extremely important that these Application Guidelines are read thoroughly before using Rust Bullet products. The selection of the […]
Contact Us

USA 1-800-245-1600
CANADA 1-800-789-3993

Support@RustBullet.com